High Temperature Corrosion Effect of Superheater Materials by Alkali Chlorides 


Vol. 24,  No. 4, pp. 339-347, Dec.  2018
10.7464/ksct.2018.24.4.339


PDF
  Abstract

In order to cope with environmental problems and climate change caused by fossil fuels, renewable energy supply is increasing year by year. Currently, waste energy accounts for 60% of renewable energy production. However, waste has a lower calorific value than fossil fuels and contains various harmful substances, which causes serious problems when applied to power generation boilers. In particular, the chlorine in the waste fuel increases slagging and fouling of boiler heat exchangers, leading to a reduction in thermal efficiency and the main cause of high temperature corrosion, lowering facility operation rate and increasing operating cost. In this study, the high temperature corrosion experiments of superheater materials (ASME SA213/ASTM A213 T2, T12 and T22 alloy steel) by alkali chlorides were conducted, and their corrosion characteristics were analyzed by the weight loss method and SEM-EDS. Experiments show that the higher the temperature and chloride content, the more corrosion occurs, and KCl further corrodes the materials compared to NaCl under the same condition. In addition, the higher the chromium content of the material, the better the corrosion resistance to the alkali chlorides.

  Statistics
Cumulative Counts from November, 2022
Multiple requests among the same browser session are counted as one view. If you mouse over a chart, the values of data points will be shown.


  Cite this article

[IEEE Style]

K. BJ, J. SH, K. HS, R. CK, L. UD, "High Temperature Corrosion Effect of Superheater Materials by Alkali Chlorides," Clean Technology, vol. 24, no. 4, pp. 339-347, 2018. DOI: 10.7464/ksct.2018.24.4.339.

[ACM Style]

Kim BJ, Jeon SH, Kim HS, Ryu CK, and Lee UD. 2018. High Temperature Corrosion Effect of Superheater Materials by Alkali Chlorides. Clean Technology, 24, 4, (2018), 339-347. DOI: 10.7464/ksct.2018.24.4.339.