A Study on the Water-soluble Fiber at the Room Temperature using Carboxymethylcellulose(CMC) Synthesis 


Vol. 11,  No. 2, pp. 105-116, Jun.  2005


PDF
  Abstract

Carboxymethylcellulose(CMC) which is water soluble at room temperature was manufactured from the cellulose material in this study. Experimental parameters were reaction temperature, time and concentration of NaOH and monochloroacetic acid. CMC was tested for solubility, degree of substitution(D.S.) and tensile strength. The surface structure of CMC fiber was tested using scanning electron microscope(SEM). CMC manufactured from viscose rayon was affected by the chemical concentration rather then the reaction time and temperature. Also, degree of substitution is closely related to the solubility of the CMC.

  Statistics
Cumulative Counts from November, 2022
Multiple requests among the same browser session are counted as one view. If you mouse over a chart, the values of data points will be shown.


  Cite this article

[IEEE Style]

S. HJ, C. Y, P. JW, "A Study on the Water-soluble Fiber at the Room Temperature using Carboxymethylcellulose(CMC) Synthesis," Clean Technology, vol. 11, no. 2, pp. 105-116, 2005. DOI: .

[ACM Style]

Song HJ, Choi Y, and Park JW. 2005. A Study on the Water-soluble Fiber at the Room Temperature using Carboxymethylcellulose(CMC) Synthesis. Clean Technology, 11, 2, (2005), 105-116. DOI: .